Learn how to remove loose mortar on brick steps and repoint the joints with fresh mortar. A beginner-friendly guide to safer, sturdier outdoor entry steps.

Published · Last updated
Short on time?

Jump to the 30-second cheat sheet for the key points.

Jump to cheat sheet ↓

One little fix at a time, we'll make your house a home! If your brick steps are dropping sandy crumbs, showing gaps, or wobbling at the edges, the mortar joints are likely failing. Repointing means removing the loose old mortar and packing in new mortar so the bricks are supported again.

It can be beginner-friendly when the steps are structurally sound and you are repairing joints, not rebuilding the staircase. Since steps are safety-critical, take your time and do a careful reality check before you start.

A close-up photo of outdoor brick steps with cracked and missing mortar joints between bricks, showing loose sandy mortar and small gaps

Before you start

Repointing is perfect when the bricks are mostly sound but the joints are cracked, powdery, or missing.

Repointing is a good fit if

  • Mortar crumbles when you scrape it with a screwdriver.
  • Joints have hairline cracks that have widened over time.
  • Small sections are missing and collecting water.
  • Bricks feel stable but the joints look tired.

Plan a bigger repair if

  • Steps are sinking, tilting, or pulling away from the house.
  • Multiple bricks are loose, rocking, or broken through the step body.
  • There are wide structural cracks that run through bricks, not just the joints.
  • You see major movement after freeze-thaw seasons.

If water is the root cause, it is worth checking drainage too. Keeping water away from masonry helps your new mortar last longer. A simple upgrade like downspout extensions can reduce splash and saturation near entry steps.

Tools and materials

Safety

  • Safety glasses (chips fly when you chisel mortar)
  • Dust mask or respirator (mortar and masonry dust are gritty and irritating)
  • Work gloves
  • Hearing protection if using power tools

Mortar removal and prep

  • Cold chisel and hammer (or a masonry chisel)
  • Pointing trowel
  • Joint raker tool or carbide grout saw (helpful for tight joints)
  • Stiff nylon brush
  • Shop vacuum or hand broom
  • Spray bottle or small pump sprayer (clean water)

Repointing materials

  • Mortar mix suitable for brick (see mortar notes below)
  • Clean bucket and mixing tool
  • Margin trowel for mixing and loading
  • Mortar bag or jointer tools (optional but helpful)
  • Sponge and clean rags

Beginner caution about grinders: Avoid using an angle grinder for mortar removal on brick steps unless you already know what you are doing. It is very easy to scar brick faces and widen joints, and the dust can be serious.

Masonry hand tools laid on a work surface, including a pointing trowel, jointer tools, a cold chisel, and a stiff brush

Step 1: Pick the right day

Mortar needs gentle conditions to cure well.

  • Aim for mild weather: roughly 40°F to 80°F is a comfortable range for many mortar mixes.
  • Avoid direct blazing sun and wind if possible. Fast drying weakens mortar.
  • Plan for a dry window: avoid rain during the first 24 to 48 hours if you can. A light mist is not the same as a soaking storm, but fresh joints still need protection.

Always check the specific instructions on your mortar bag because curing recommendations can vary.

Step 2: Check how deep to go

Use a screwdriver or the tip of a pointing trowel to probe a few joints. If only the surface is dusty, you still need to remove enough depth for the new mortar to grip.

  • Rule of thumb: remove loose mortar to about 2 times the joint width.
  • Practical range: on many brick steps, that often works out to roughly 1/2 inch to 3/4 inch, but let the joint width and what you find in the wall guide you.
  • Real goal: keep removing until you hit firm, sound mortar that does not crumble.

Step 3: Chisel out loose mortar

This is the step that makes or breaks the finished look. Slow and steady protects the brick edges.

How to remove mortar without damaging bricks

  1. Put on eye protection and a mask. Mortar chips and dust happen immediately.
  2. Start with the bed joints (the horizontal joints). Angle the chisel so it bites into mortar, not the brick.
  3. Use light taps instead of big swings. Bricks chip when the tool slips.
  4. Switch to vertical joints (head joints) after the horizontals.
  5. Stop when mortar is firm. You are not trying to excavate good mortar.

Beginner tip: Keep your chisel centered in the joint. The brick corners are the easiest place to scar, and those scars tend to show forever.

A gloved hand using a cold chisel and hammer to remove crumbling mortar from a brick step joint

Step 4: Clean the joints

Mortar sticks best to clean, dust-free surfaces.

  1. Brush out the joints with a stiff nylon brush.
  2. Vacuum or sweep out all dust and crumbs.
  3. For stubborn grains on the edges, brush again or give a gentle tap with your chisel to dislodge them, taking care not to chip the brick.

If you leave dusty residue behind, the new mortar can debond and pop out later.

Step 5: Dampen the brick

Dry brick is thirsty. If it sucks water out of your fresh mortar too quickly, the mortar cures weak and chalky.

  • Mist the joints and surrounding brick until the surface looks damp, not dripping.
  • Wait a few minutes, then mist again if the masonry dries fast.

What you want: a cool, damp surface that will not pull moisture out of the new mix right away.

Step 6: Mix mortar

Follow the bag directions, then use this simple consistency check.

  • Target texture: like creamy peanut butter, not soup and not dry crumbs.
  • If it slumps off your trowel, it is too wet. If it will not pack into the joint, it is too dry.

Mix small batches. Beginners tend to work slower, and mortar that starts to stiffen in the bucket is harder to tool and bond well.

Step 7: Pack the joints

The goal is a joint that is fully filled and well compressed. Gaps inside the joint invite water.

Work in small sections: for most DIYers, a short stretch at a time (think a few feet of joint, not the whole staircase) makes it much easier to tool at the right moment.

Method A: Pointing trowel

  1. Load a small amount of mortar onto a pointing trowel.
  2. Press mortar into the joint firmly, pushing it back into the cavity.
  3. Fill in layers if the joint is deep. Pack the first layer, let it firm up slightly, then add more.
  4. Slightly overfill the joint so you can tool it to a clean finish.

Method B: Mortar bag

A mortar bag works like a sturdy pastry bag. Fill it partway, twist the top, then squeeze mortar into the joint. You still need to compact it with a jointer or trowel tip.

Mortar being squeezed from a mortar bag into the horizontal joints of outdoor brick steps

Step 8: Tool the joints

Tooling compresses the mortar surface and shapes it so rain runs off instead of sitting in the joint.

  • Wait for the right moment: when the mortar is thumbprint firm. If you tool too early, it smears. Too late, it crumbles.
  • Match the existing look if possible. Concave joints are common and durable for exterior work.
  • Brush lightly after tooling once mortar has firmed a bit more. This removes crumbs and softens edges.

Step 9: Clean the brick face

Mortar haze is easiest to avoid, and harder to fix once cured.

  • As you work, keep a damp sponge handy, but do not flood the joints.
  • Wipe stray mortar off brick faces while it is still fresh.
  • After tooling, let the mortar set a bit more, then use a dry soft brush to whisk off crumbs.

Avoid aggressive wet scrubbing early on. It can pull cement to the surface and weaken the joint edges.

If you do end up with stubborn haze, avoid rushing to strong cleaners. Do not use acidic cleaners on fresh mortar, and wait until the mortar is fully cured before using any specialty product.

Step 10: Cure the mortar

Mortar gains strength as it cures. The first couple days matter a lot.

  • Keep it slightly damp for a day or two if conditions are hot, dry, or windy. A light mist helps.
  • Protect from heavy rain for 24 to 48 hours (longer if conditions are cool and damp) so fresh joints do not wash out. If needed, use plastic sheeting tented so it does not touch the mortar.
  • Stay off the steps as long as you reasonably can, at least 24 to 48 hours. Longer is better if the steps are a main walkway.

Picking mortar

Mortar should be compatible with your brick and the existing mortar. Outdoor steps need durability, but mortar that is too hard can be a problem for softer, older bricks because the brick can crack before the joint does.

  • Common choice for many above-grade exterior brick projects: Type N is often used because it balances strength and flexibility.
  • Heavier exposure situations: brick steps can see high saturation and de-icing salts. In some builds and regions, a higher-strength mortar or a purpose-made repair mortar may be used. The best match is usually the one that fits what is already there and how the steps are built.
  • Older homes and softer brick: if your home is older (especially pre-1940) or the existing mortar is very soft and lime-rich, consider having the mortar matched or getting advice from a masonry supplier before you repoint large areas.

Color matching tip: The same mortar can look different when it dries. If a close match matters, make a tiny test batch and let it cure before doing the whole staircase.

Troubleshooting

New mortar is cracking right away

  • Likely causes: too dry a mix, joints not dampened first, or drying too fast in sun and wind.
  • Fix: remove loose cracked sections and repoint again, then mist and protect from rapid drying.

Mortar is falling out after it cures

  • Likely causes: dusty joints, not enough removal depth, or poor compaction.
  • Fix: rake out to firm mortar, clean thoroughly, repoint and tool again.

Mortar smeared on brick faces

  • Likely causes: tooling too early or wiping with a very wet sponge.
  • Fix: let smears firm up, then brush gently. For cured haze, specialty cleaners exist, but they can damage brick if misused. Start with the gentlest method first, and avoid acids on new mortar.

Joints look uneven

  • Likely causes: inconsistent fill height or tooling timing.
  • Fix: work in smaller sections so you can tool at the same firmness stage.

Help your repair last

  • Control water: extend downspouts and avoid constant splash onto the steps. See downspout extension ideas.
  • Do not seal problems in: sealing brick and mortar can trap moisture if the system is not meant to be sealed. If you are considering sealers, check whether your masonry needs to breathe.
  • Use de-icer carefully: some ice melts and repeated freeze-thaw cycles can be rough on masonry.
  • Inspect each spring and fall: small cracks are easier to repoint than big missing sections.

When to call a mason

Repointing is a great skill-builder, but steps carry weight and take weather from every angle. Consider a pro if:

  • Bricks are loose or the step structure is shifting.
  • You suspect the steps were built with the wrong mortar and are spalling or popping.
  • You need rebuilding, not just joint repair.

That said, if your bricks are solid and the joints are just tired, repointing is a sturdy, satisfying weekend win.

The 30-second cheat sheet

The key points from this guide, in one place.

  • Repointing goal: Remove loose mortar and replace it so brick steps feel solid and shed water properly.
  • Remove enough old mortar: A good rule of thumb is about 2 times the joint width, and always stop at firm, sound mortar.
  • Go slow with the chisel: Light taps, keep the tool centered in the joint to avoid chipping brick edges.
  • Clean matters: Brush and vacuum joints so new mortar bonds to masonry, not dust.
  • Dampen first: Mist brick and joints so dry masonry does not steal water from fresh mortar.
  • Mix consistency: Like creamy peanut butter. Mix small batches so it does not stiffen in the bucket.
  • Pack and compress: Fill joints fully, in layers if needed, then tool when mortar is thumbprint firm.
  • Cure gently: Protect from heavy rain, avoid fast drying, and keep off the steps 24 to 48 hours if possible.
  • Red flags: Steps sinking, bricks rocking, or big structural cracks usually mean repair beyond repointing.